Weldable Alumina Tiles
Weldable Alumina Tiles
A standard ceramic tile bonded with epoxy works fine on a flat, static surface with low impact. But put it on a crusher discharge chute where rocks drop from height, or on a vibrating feeder where the whole structure shakes, and eventually that tile will come loose. The epoxy doesn't fail instantly. It fatigues over weeks or months. Then one day you find a tile missing, a hole in the lining, and the steel underneath already worn halfway through.
Tecera makes a different version. It's the same high‑density alumina ceramic – 95% Al₂O₃, Mohs hardness 9, water absorption below 0.01% – but with a steel stud embedded in the back. A hole through the center lets a welding gun reach that stud. You weld the tile directly to the steel shell. No waiting for epoxy to cure. No risk of the adhesive failing from impact or heat. The tile stays where you put it until you grind the weld off.
This isn't a product for every application. If you're lining a static chute with fine, low‑velocity material, standard epoxy tiles are cheaper and easier. But if you have heavy impact, constant vibration, high temperature (above 150°C), or a plant that can't afford 24 hours of downtime for adhesive to cure, the weldable version makes sense.
What you're actually getting
The tile itself is nothing exotic. It's the same 95% alumina we use in our standard liners. Bulk density around 3.68 g/cm³, which is high enough that there's virtually no open porosity. That matters because porosity leads to two problems: liquid absorption (which causes freeze‑thaw cracking in cold climates) and chemical attack (acidic slurry seeping into the tile). With water absorption at or below 0.01%, neither happens.
The difference is in the back face. A countersunk hole – typically 6‑8mm diameter at the narrow end, wider at the surface – goes through the tile. A steel stud, coated with a thin layer of copper for better weld consistency, sits in that hole. The stud is positioned during tile pressing, not added later. That matters because drilling a hole after sintering would create micro‑cracks around the edge, and those cracks would grow under impact.
The welding process is straightforward. A stud welding gun – the same type used to attach studs to steel beams in construction – clamps onto the stud. The gun pulls the stud slightly away from the steel surface, strikes an arc, melts the stud tip and the steel beneath, then pushes the stud into the molten pool. The whole cycle takes about 0.2 seconds. The ceramic hole is sized to keep the arc away from the tile edges, so the heat doesn't crack the ceramic.
Where people actually use these
The most common application is crusher discharge chutes in hard rock mining. Copper, gold, iron ore. The material coming out of a primary crusher is a mix of coarse lumps and fine particles, dropping from height onto the chute. Standard epoxy‑bonded tiles tend to pop off at the impact points. The weldable tiles don't. One copper mine in Chile replaced their chute liners every 6‑8 months with epoxy tiles. They switched to weldable tiles three years ago. The same set is still there.
Another common use is coal chutes in prep plants, especially where the coal is wet. Wet coal is sticky. It builds up on rough surfaces. When the chute gets blocked, someone has to go in with a bar or a water hose to clear it. That cleaning process knocks tiles loose. Weldable tiles survive that abuse better because they're mechanically fixed, not just glued.
Power plants use them in coal pulverizer feed chutes. The coal is dry but abrasive. The chute vibrates constantly from the pulverizer below. Vibration is hard on epoxy joints – the repeated small movements eventually break the bond. Welded joints don't care about vibration.
Steel mills use them in sinter plant chutes. Sinter is hot – 200‑300°C when it leaves the strand. Most epoxies soften at those temperatures. Weldable tiles with no adhesive underneath (just the weld) handle the heat fine.
Technical Specifications
The table below shows typical specifications for Tecera's weldable alumina tile grades. Values are based on internal testing and industry standards; batch certificates are available on request.
| Property | 92% Alumina Grade | 95% Alumina Grade | ZTA Grade |
|---|---|---|---|
| Al₂O₃ content (%) | ≥92 | ≥95 | 70–80 |
| ZrO₂ content (%) | - | - | 20–30 |
| Bulk density (g/cm³) | ≥3.63 | ≥3.68 | ≥4.00 |
| Water absorption (%) | ≤0.01 | ≤0.01 | ≤0.01 |
| Mohs hardness | 9 | 9 | 9 |
| Vickers hardness (HV) | 1000–1100 | 1150–1250 | 1300–1400 |
| Fracture toughness (MPa·m¹/²) | 3.5–4.0 | 3.5–4.0 | 5.0–6.5 |
| Bending strength (MPa) | ≥240 | ≥250 | ≥400 |
| Maximum service temperature (°C) | 1200 | 1250 | 1450 |
Available tile sizes and shapes:
| Shape | Length (mm) | Width (mm) | Thickness (mm) | Hole diameter (mm) |
|---|---|---|---|---|
| Square (plain) | 50, 100, 150 | 50, 100, 150 | 10, 12, 15, 20, 25 | 6–8 (countersunk) |
| Square (weldable) | 50, 100, 150 | 50, 100, 150 | 10, 12, 15, 20, 25 | 6–8 (countersunk) |
| Rectangle | 150 | 50, 75, 100 | 10, 12, 15, 20, 25 | 6–8 (countersunk) |
| Trapezoid | 150 | 50 (top), 45 (bottom) | 10, 12, 15, 20, 25 | 6–8 (countersunk) |
| Half‑tile | 75 | 50 (top), 45 (bottom) | 10, 12, 15, 20, 25 | 6–8 (countersunk) |
Custom sizes, shapes, and thicknesses are available on request.
A few numbers for reference
We make two standard grades for weldable tiles. Both are available in thicknesses from 10mm to 25mm, in square (50, 100, 150mm) and trapezoid shapes.
95% alumina: Al₂O₃ ≥95%, density ≥3.68 g/cm³, water absorption ≤0.01%, Vickers hardness 1150‑1250, fracture toughness about 3.5‑4.0 MPa·m¹/². This covers most applications.
ZTA (zirconia‑toughened alumina): Al₂O₃ 70‑80%, ZrO₂ 20‑30%, density ≥4.00 g/cm³, fracture toughness 5.0‑6.5 MPa·m¹/². About 50% tougher than standard alumina. We recommend this for high‑impact zones like the feed point of a primary crusher chute.
The stud size depends on tile thickness. For 10‑12mm tiles, we use 6mm studs. For 15‑20mm tiles, 8mm studs. For 25mm tiles, 10mm studs. The stud length is matched to the tile thickness so the tip sits just below the tile surface before welding.
Installation – what's involved
You need a stud welding gun, a clean steel surface, and a power source. The steel doesn't need to be perfectly flat, but it does need to be free of rust, oil, and thick scale. A grinder with a flap disc is usually enough.
The process: dry‑fit the tiles first to check the layout. Apply a thin layer of epoxy to the back of each tile if you want additional bonding – this is optional but recommended for impact areas. Press the tile into place. Insert the welding gun through the hole, engage the stud, pull the trigger. That's it. Move to the next tile.
For repairs, you can replace individual tiles. Grind off the old stud flush with the steel surface. Weld the new tile over the same spot. The whole repair takes a few minutes.
The main limitation is access. The welding gun needs to fit over the tile, so you need clearance above the surface. For confined spaces, there are right‑angle stud welding guns, but they're less common.
What it costs
A weldable tile costs more than a plain tile. The stud adds material cost, and the countersunk hole adds a forming step. But the total installed cost – including labor – is often lower because you don't wait for epoxy to cure. For a large chute, the difference in material cost might be 30‑40% higher. But if that chute would have failed after six months with epoxy tiles and lasts three years with welded tiles, the math works out.
We don't claim weldable tiles last forever. They don't. The ceramic still wears. But they don't fall off. That's the key difference. The failure mode changes from "tile popped off and left exposed steel" to "ceramic slowly wore down over years." The first is unpredictable and requires emergency repair. The second is predictable and can be scheduled.
When not to use them
A few situations where weldable tiles aren't the right answer.
If the steel shell is thin – less than 3mm – the welding heat can warp it. For thin liners, epoxy or mechanical fasteners are better.
If the chute has complex curves or tight corners, weldable tiles are harder to fit because the welding gun needs straight access. In those spots, use epoxy tiles or a castable ceramic.
If the plant doesn't have a stud welding gun, buying one adds cost. The guns aren't expensive – a basic model is a few hundred dollars – but if you only need to do one small repair, it might not be worth it.
Sizing and ordering
We make weldable tiles in square and trapezoid shapes. Square tiles go down fast. Trapezoid tiles stagger the seams, which prevents continuous wear grooves. For high‑wear applications, we recommend trapezoid.
Standard thicknesses: 10, 12, 15, 20, 25mm. For anything thicker than 25mm, we can custom‑press. Lead time for custom sizes is about 4‑6 weeks.
We supply tiles in boxes of 50 or 100. For large projects – over 500 tiles – we offer bulk pallet pricing. Samples are available. If you want to test the welding process before buying a full set, we'll send a small batch for free.
For a quote, send us the tile size, thickness, grade (95% or ZTA), quantity, and delivery address. If you have a drawing of the chute or hopper, include it – we can help with the layout and suggest tile patterns that minimize gaps. Response time is usually 24‑48 hours.
Hot Tags: weldable alumina tiles, China weldable alumina tiles manufacturers, suppliers, factory, Ceramic Tile Liner, coal hopper iner, ceramic feeder liner, trapzoid ceramic tile, industrial ceramic lining, alumina ceramic tile